Pb99.94 or PB940R is a pure substance that has a purity of 99.94 percent and is used for a wide variety of applications.
Delivery forms
Ingots with or without suspension
Rods type 3K & 4K
Solid wires
Pellets (hemisphere sections)
Sticks® (cylinder)
Other formats or products not listed here may be possible by arrangement.
Applications
This soft lead is a pure substance, which is primarily used for the following applications:
Balancing weights
Castings for accumulators
Aggregate for galvanizing and steel production
Radiation protection
Hand soldering
Dip tinning
Products
Pellets made from Pb99,94
6829
molded
none
without
Pellets
Pellets
6 mm
18 mm
9133
molded
none
without
Pellets
Pellets
12 mm
25 mm
9132
molded
none
without
Pellets
Pellets
10 mm
27 mm
The products shown are only a selection from our product range. Please contact us for your desired configuration of Pellets from Pb99,94.
Blocks made from Pb99,94
1272
molded
none
without
Block
Blocks
725 mm
465 mm
310 mm
2766
molded
none
without
Block
Blocks
725 mm
465 mm
310 mm
The products shown are only a selection from our product range. Please contact us for your desired configuration of Blocks from Pb99,94.
Sticks made from Pb99,94
1476
molded
none
without
square cut
Sticks
340 mm
30 mm
20 mm
1386
molded
none
without
triangular
Sticks
400 mm
10 mm
10 mm
The products shown are only a selection from our product range. Please contact us for your desired configuration of Sticks from Pb99,94.
Studs made from Pb99,94
1191
molded
none
without
Studs
Studs
172 mm
71 mm
7374
molded
none
without
Studs
Studs
180 mm
55 mm
The products shown are only a selection from our product range. Please contact us for your desired configuration of Studs from Pb99,94.
Ingots made from Pb99,94
1474
molded
none
without
Ingot Type H
Ingots
420 mm
115 mm
30 mm
The products shown are only a selection from our product range. Please contact us for your desired configuration of Ingots from Pb99,94.
Material properties
| Melting temperature °C | 296-301 |
| Solder wave temperature °C | n.s. |
| Density g/cm³ | 11.34 |
| Hardness HB | n.s. |
| Tensile strength N/mm² | 12 |
| Stretching % | n.s. |
| Specific heat of fusion J/g | n.s. |
| Electrical conductivity μΩm | n.s. |
This alloy can be stored for at least 48 months if properly stored in a clean and dry environment. For massive formats, further processing is usually possible after the specified storage period has expired but should be technically checked and approved in advance.
Chemical composition according EN 12659
(Data in percent by weight)
| Element | Formula sign | Composition |
|---|---|---|
| Lead | Pb | Residue |
| Bismuth | Bi | < 0.06 |
| Silver | Ag | < 0.008 |
| Copper | Cu | < 0.005 |
| Antimony | Sb | < 0.001 |
| Arsenic | As | < 0.001 |
| Tin | Sn | < 0.001 |
| Cadmium | Cd | < 0.002 |
| Nickel | Ni | < 0.002 |
| Zinc | Zn | < 0.0005 |
The data given in the table are based on the standardization data of the EN12659.